Fiber Reinforced Plastics/Composites ›› 2019, Vol. 0 ›› Issue (1): 71-74.

• APPLICATION RESEARCH • Previous Articles     Next Articles

STUDY ON METAL SANDBLASTING PROCESS FOR BONDING OF COMPOSITES

ZHANG Yu-jie1,2, ZHAO Xin1,2, GUO Jin-hai1,2, SHI Wen-feng1,2   

  1. 1.Shanghai Composite Materials Technology Co., Ltd., Shanghai 201112, China;
    2.Shanghai Engineering Research Center of Aerospace Resin Based Composite, Shanghai 201112, China
  • Received:2018-04-28 Online:2019-01-28 Published:2019-01-28

Abstract: The paper introduces metal materials and their surface treatment for bonding of composites, and tests the sandblast parameters of TC4 titanium alloy, 5052 aluminum alloy, 304 stainless stell and 4J36 invar stell. Taking sandblast time as variable as well as tensile shear strength between metal and composite after bonding to verify the surface condition under metal sandblasting. The test demonstrates that appropriate sandblasting parameter of TC4 titanium alloy is 30 s±5 s/15 cm2 and 20 s±5 s/15 cm2 for 052 aluminum alloy, 45 s±5 s/15 cm2 for 304 stainless stell, 25 s±5 s/15 cm2 for 4J36 invar stell under the condition of 40 mesh quartz sand, the sandblasting distance of 150 mm, the sandblasting angle of 45°, the sandblasting pressure of 0.5 MPa.

Key words: sandblast, bonding, metal, composite

CLC Number: